After we've done the sanding/lacquering for several layers, today is our final layer. The 15th layers!!
We remind our step.
Apply 400 grit water proof sanding paper, 1st lacquer, wait for at least 8 hours, 2nd lacquer...
Apply 400 grit water proof sanding paper, 3rd lacquer, wait for at least 8 hours, 4th lacquer...
Apply 400 grit water proof sanding paper, 5th lacquer, wait for at least 8 hours, 6th lacquer...
....
 Until we finish 14th
Apply 500 grit water proof sanding paper, apply 800 grit water proof sanding paper, 15th lacquer

Here are some of our 800 grit result (before 15th lacquer layer)









After 15th lacquer layers..